Your location:Home page >>Products  
      Product list
      UV nail gel
      UV gels
      Package size
      Colors
      Color chart
      LED light
      Electronic Technology
      Touch screen
      LCD & LCM module
      The reinforcement of electronic cable and welding joint
      Surface coating
      Sealing of Electronic materials
      UV anaerobic metal joint
      Plastic Technology
      PET & APET
      Surface-dry Glue for plastics
      General-purpose plastics
      Medical instruments
      buttons on mobile phone
      Glass & Metal
      Crystal and Glass adhesive
      Glass and Metal adhesive
 
        Glass and Metal adhesive


 UV adhesive for glass bond metal 

Item No.

Products' features and typical usage

3212

Flexibility and stability formula, have a good adhesion to many kinds of metals, such as stainless steel, aluminum alloy, electroplated coating, special glass and crystal. no white, no bubbles and won’t fall/peel off after curing, also with excellent aging-resistance performance. Typically used in the making of glass,tea table, dining table and lighting fixture, etc.

3213

3216

3217

High flexibility formula, no white, no bubbles and won’t fall/peel off after curing, also with excellent aging-resistance performance. Typical applications in the bonding of aluminum & steel plate & glass on the electronic scales.

3218

3205

3223

Fast curing, the surface can be totally and nicely dried, excellent waterproof performance, and have a good adhesion to glass, crystal and all kinds of metal. Typical applications in the glass and aluminum alloy adhesion of security camera lens, etc.

3224

Status

Parameters Name

Technical Parameters

3212

3213

3216

3217

3218

3205

3223

3224

 

Before UV curing

Liquid Color

Clear light yellow liquid

Clear light yellow liquid

Clear light yellow liquid

Clear light yellow liquid

Clear light yellow liquid

Clear light yellow liquid

Clear light yellow liquid

Clear light yellow liquid

Viscosity(cps, tested under 25)

750-1000

550-700

4500-6000

560-600

1800-2000

1800-3000

5500-6500

12000-18000

Proportion (g/cm3)

1.03

1.03

1.03

1.03

1.03

1.03

1.03

1.05

PH value

6.5

5.0

5.0

5.0

5.0

5.0

6.5

6.0

During UV curing

setting time/sec'

10

10

14

20

16

11

4

3

Solid energy (mj/cm2)

1500

1500

1500

1500

1500

1500

500

800

After UV curing

Hardness

Shore A

/

/

/

75

50

/

/

/

Shore D

78

58

65

/

/

36

80

82

Pencil

/

/

/

/

/

/

/

/

Shrinkage rate(%)

3

3

3

2

2

3

3.5

3.5

Bibulous rate(%)

1.5

3

3

3

3

2

1.5

1.5

temperature-resistant scope(℃)

-5~150

-5~150

5~150

-5~150

-5~150

-5~150

-5~150

-5~150

Solid content(%)

100%

100%

100%

100%

100%

100%

100%

100%

Tensile strength (MPa)

24

18

18

18

18

22

15

15

Shear strength

/

/

/

/

/

/

/

/

Peel strength (Kgf/cm2)

26

20

20

20

20

23

/

/

Elongation at break

/

/

/

/

/

/

/

/

Light transmittance (%)

/

/

/

/

/

/

/

/

Refractive index

/

/

/

/

/

/

/

/

Elastic modulus

/

/

/

/

/

/

/

/

Dielectric constant (1MHz)

3.2

3.2

3.2

3.2

3.2

3.2

3.2

3.2

Dielectric loss(1MHz)

0.03

0.03

0.03

0.03

0.03

0.03

0.03

0.03

Dielectric strength (KV/MM)

20

20

25

25

25

20

20

20

Surface resistivity(Ω.cm)

0.8 x 1016

0.8 x 1016

0.8 x 1016

0.8 x 1016

0.8 x 1016

0.8 x 1016

0.8 x 1016

0.8 x 1016

Volume resistivity(Ω.cm)

0.5 x 1016

0.5x 1016

0.5 x 1016

0.5 x 1016

0.5 x 1016

0.5x 1016

0.5 x 1016

0.5x 1016

Spec

250ml/bottle

Shelflife

One Year(Seal storage and comply with storage conditions.)

Notes

1. Storage under 8℃25℃, in the dark, sealing, ventilation, cool conditions, and far away from children.

2. Keep air ventilation when using, and take the safe protection measures, such as don't use your skin to touch the resin directly or longly.

Remarks

1.) Viscosity standard Tested under 25±0.5, by using the container with diameter 6-7cm, and height 10cm.

2.) The setting time of above items were tested under the condition of glass bond glass  with 40w and light intensity is under 7.5mW/cm2.                                                                                                                                           3.) Above tensile & shear strength data tested when glass bond glass, glass bond crystal.

4.) Other test parameters are tested on the basis of the national testing.